STREAKING OR DIE LINES

Recommended Actions

Contaminated or degraded resin • See “Dirt and Contamination” Burned-out heater band, blown fuse or bad • Replace bad component. contactor stuck on/off. Heater band loose or plastic lodged between • Clean metal surface and heater band heater band and metal surface. and retighten (recheck tightness after zone has reached operating temperature) Carbonized or degraded resin in head • Disassemble and clean. Foreign matter lodged in head tooling • Repair/replace tooling if necessary • Plate head tooling for best finish. Damaged head tooling • Repair/replace tooling if necessary • Plate head tooling for best finish
  • Contaminated or degraded resin
  • See “Dirt and Contamination” Burned-out heater band, blown fuse or bad
  • Replace bad component. contactor stuck on/off.
  • Heater band loose or plastic lodged between
  • Clean metal surface and heater band heater band and metal surface. and
  • retighten (recheck tightness after zone has reached operating temperature)
  • Carbonized or degraded resin in head
  • Disassemble and clean.
  • Foreign matter lodged in head tooling
  • Repair/replace tooling if necessary
  • Plate head tooling for best finish.
  • Damaged head tooling
  • Repair/replace tooling if necessary
  • Plate head tooling for best finish