UNMELTED PELLETS IN PART

Recommended Actions

Melt not homogeneous • Increase backpressure by choke adjustment • Use finer screen pack • Check for screw/barrel wear and ensure proper screw is being used for the application Melt temperature too low • Allow more time for machine heat-up • Increase melt temperature • Check for bad heater bands, blown fuse, or bad contactor and replace bad component. Cycle too fast • Reduce cycle time.
  • Melt not homogeneous
  • Increase backpressure by choke adjustment
  • Use finer screen pack
  • Check for screw/barrel wear and ensure proper screw is being used for the
  • application
  • Melt temperature too low
  • Allow more time for machine heat-up
  • Increase melt temperature
  • Check for bad heater bands, blown fuse, or bad contactor and replace bad
  • component.
  • Cycle too fast
  • Reduce cycle time.