WEBBING

Recommended Actions

Incorrect mold position • Relocate mold relative to parison. Incorrect parison size • Adjust push-out speeds • Change tooling • Use material with lower die swell Inner parison walls touching • Use pre-blow. • Add pinch bars and/or pre-pinch bars • Adjust clamp speed.
  • Incorrect mold position
  • Relocate mold relative to parison.
  • Incorrect parison size
  • Adjust push-out speeds
  • Change tooling
  • Use material with lower die swell
  • Inner parison walls touching
  • Use pre-blow.
  • Add pinch bars and/or pre-pinch bars
  • Adjust clamp speed.