Injection Injection Molding
Delaminating
Recommended Actions
Delaminating occurs when single surface layers start flaking off the molded part.
Possible Solutions
Adjust injection speed.
Check for material contamination. Incompatible resins or colorants may have been accidentally mixed causing this condition to be seen.
Dry material.
Increase the melt temperature.
Increase mold temperature.
Insufficient Blending, Check the melt homogeneity and plasticizing performance.
- Delaminating occurs when single surface layers start flaking off the molded part.
- Possible Solutions
- Adjust injection speed.
- Check for material contamination. Incompatible resins or colorants may have been accidentally mixed causing this condition to be seen.
- Dry material.
- Increase the melt temperature.
- Increase mold temperature.
- Insufficient Blending, Check the melt homogeneity and plasticizing performance.