Injection Injection Molding

Splay Marks, Silver Streaks.

Recommended Actions

Possible Solutions Check for contamination. Decrease the melt temperature. Decrease nozzle temperature. Dry resin pellets before use. As per the manufacturers recommendations Incorrect storage of pellets Moisture on the pellets could be transferred into the melt, especially if the resin is not normally pre-dried. Raise the mold temperature. This will prevent condensation on the mold walls from being carried into the melt. Ensure the mold is not leaking water onto the cores or cavities. Again this will prevent condensation on the mold walls from being carried into the melt. Relocate gates on or as near as possible to thick sections. Shorten overall cycle.
  • Possible Solutions
  • Check for contamination.
  • Decrease the melt temperature.
  • Decrease nozzle temperature.
  • Dry resin pellets before use. As per the manufacturers recommendations
  • Incorrect storage of pellets Moisture on the pellets could be transferred into the melt, especially if the resin is not normally pre-dried.
  • Raise the mold temperature. This will prevent condensation on the mold walls from being carried into the melt.
  • Ensure the mold is not leaking water onto the cores or cavities. Again this will prevent condensation on the mold walls from being carried into the melt.
  • Relocate gates on or as near as possible to thick sections.
  • Shorten overall cycle.

Related Knowledge

Source

Imported from Molding Defects All Platforms spreadsheet

We use first-party analytics to understand which tooling topics are most valuable to our visitors. This helps us improve content and is never shared with advertisers. See our Privacy Policy and Cookie Policy.