Injection Stretch Blow Injection Stretch Blow Molding (ISBM)

LONG GATES

Recommended Actions

Improper process temperatures. • Raise the temperature in gate area of mold. • Verify the hot manifold temperature controller is operating correctly. • Check for loose thermocouple in hot manifold.
  • Improper process temperatures.
  • Raise the temperature in gate area of mold.
  • Verify the hot manifold temperature controller is
  • operating correctly.
  • Check for loose thermocouple in hot manifold.